liquid stringer
A technique for creating lines with glass.
Liquid stringer used a mixture of glass powder and a glue-like medium that can be squeezed from a plastic bottle or pastry bag and tip.
Richard LaLonde (credited by many as the originator for this technique) has a recipe for liquid string that can be found in our recipe section.