Step 3: Understanding the Double Slump
Now for the tricky (but not difficult) part: folding the top of the glass over to make a channel for the cord or chain - without using a torch or reaching into the kiln while it is hot.
The secret is slumping the glass not once, but twice!
The first slump - which is done face down hanging off the end of a piece of fiber-board - bends the glass like this:
We then flip the glass over bend the glass like this in a second slump:

How does that work? The next page will show you the setup for the first bend.