This site is brought to you by Helios Kiln Glass Studio in Austin, TX.
Artists working with a combination of glass and lights?
Submitted by artglasscat on Tue, 07/10/2012 - 02:42.
Hi -
Does anyone know any contemporary fused glass artists working with a combination of glass and lights?
I'm about to undertake a research project into the combination of fused glass, lights and technology. Does anyone know of any contemporary fused glass artists who are using the new light technologies in their work?


Glass and lights
I know of no one currently doing this but I would start my search with the folks at Corning in NY
request re: your research glass/lights/tech
Not wanting to ask without providing something, I found this: http://www.finne.com/blog/?p=8
Perhaps off the mark but it does incorporate glass, tech and lighting. I found it while looking, unsuccessfully, for another site. I've been looking into LED lights for my fused glass and mixed media pieces.
Can you please share your findings?
glass and lights
There is a glass studio in Mt Rainier Maryland, the Washington Glass School, that has combined fused glass with neon lighting. you can look them up at Washingtonglassschool.com.
Merrilee
Take a look at the class
Take a look at the class Jeremy Bert is teaching at Pilchuck this summer (page 39):
http://issuu.com/pilchuckglassschool/docs/2012_summer_program_course_catalog_v2/37?mode=window&viewMode=doublePage
----------------------
Paul