Image transfer

I was plannig on attending a class at Bullseye, about image transfer with a laser printer. But it is one hour on a Sunday and it seems a bit much to drive down there from Bremerton and back for  a one hour class.  I know I have see some discussion about it in this forum (I think I even added to it). I've tried a few things and have been very unsucessful. I bought some "decal paper" and ended up with a black blob. Any guidance out there or a website to help?

0

I use the Decal paper

I use the Decal paper extensively and they are fairly simple. You should not get a blob. First, The paper is only good for laser printers. Make sure you use that.

Second be sure to remove the protective film form the decal paper before printing on it.then when it is made, but out your decal and soak it for 45seconds to 1 min and then slide it on to the glass.

Make sure you are doing the above and give it another try.

Barry Kaiser

www.kaiserglass.com

Hi Berry, which deacal paper

Hi Berry,

which deacal paper are you using? And does any laser printer work, since I have seen discussions  about laser printers and to be carful to buy just a certain kind of toner. I own a HP laser printer and got my toner from a recycle company.

petra kaiser - www.kaiserlee.com

 

Petra, I use Beldecal's

Petra,

I use Beldecal's paper. I think that they are pretty much all the same.

As to printers, you do need to use a laser toner that has Iron Oxide in sufficient concentration to create the color. All HP printers do have it. I too refill my cartridges and the refill I use works fine.

 

 

Barry Kaiser

www.kaiserglass.com

thank you for the tip, I

thank you for the tip, I just was at their web site and found the paper - is it correct, that you don't fire those deacals? Would they be scratch resistent?

petra kaiser - www.kaiserlee.com

 

You DO fire the decals. They

You DO fire the decals. They are fired into the glass.

Beldecal has several different types of paper. There is one that is used for firing. That is the one to use. Delphi and several other companies have it.

 

Barry Kaiser

www.kaiserglass.com

photosilkscreen vs. decals

Thanks for your interesting information...and for the great site of your work!

I'm wondering if you could explain the difference between photo silkscreening and
these decals
 in getting images into glass.  I'm aware they are different processes,
but I'm not clear about the differing results or expense, technique and time differences. I'm interested in working at the 2-3 ' size...would this also be appropriate in that application?  Are you familiar with this?

Thanks again,

Jolinda

Windows listen attentively for the sound of broken glass.

Image transfer paper

Barry, Thanks for the information. I got on your site and can see that you have got this process down. I got on Beldecal's website and call me dumb, but It couldn't seem to find the paper for glass or ceramic that I would actually order. Any guidance? Also, I noticed that you said you refill your own toner cartridges. Where do you get the materials and instructions? Also, is there any way that you know of to actually find out if, for instance, Samsung laser printers use the iron oxidie that is needed. I know I could/should search for this information myself, however, you seem to have the ansewers that I'm looking for, hope you don't mind. Don

Jolinda and Don, I'll try 

Jolinda and Don,

I'll try  and answer both of your questions. First, the process of making a silk screened decal is probably far beyond where you want to go. The decals we are talking about here are only the sepia colored ones made on a laser printer. The full color decals involve silk screening colors onto the paper and then covering them with gelatin.

Don, I have to agree with you about the confusion on papers.  I originally bought a large supply of the decal paper from Beldecal because I use it in two of my classes.After looking at the site, I don't know for sure which one I bought, but I think it is the regular clear laser paper. I would suggest you call them and ask.

 

Barry Kaiser

www.kaiserglass.com

Samsung printer

Don,

I am sorry, this is one answer I do not have. I don't know if the Samsung works.

 

Barry Kaiser

www.kaiserglass.com

Barry... Thanks so much for

Barry...

Thanks so much for your help and information.  You're right this is a bit complicated
from where I sit now...and your classes are just too far away from San Diego!
Thanks again for your care...

Jolinda 

Windows listen attentively for the sound of broken glass.

High or low fire decals?

Would a fellow glass-a-holic please tell me where and what kind of decals I use for fusing onto glass?  I saw some pics on the web of some great glass decals.  One that I especially liked was of a Mardis Gras face. In my searching on the web, I found pretty generic ones (dragonfly, butterfly, cross)...but nothing like that one. 

I live in the U.S.  Any suggestions out there?  Thanks!

Comment viewing options

Select your preferred way to display the comments and click "Save settings" to activate your changes.