shiny on both sides?
Submitted by maryt on Wed, 06/24/2009 - 22:34.
I want to hang some fused glass pieces in the windows, but they're only pretty to look at on one side. Is it possible to get fused glass to be shiny on both sides?


Yes. The longer answer is
Yes.
The longer answer is that you have to grind the surface smooth, then go down in grits and finally polish. Probably not worth it for a window hanging.