I have been making initial jewlery with dichroic glass.  I am doing etching.  I put on a decal for the ititial then do etching.  I feel like I am wasting good dichroic though. The only thing left of the dichroic is the actual letter.  Any ideas to help do the reverse? Maybe decals that are letters that I can fire?  Where to get them?

You can buy some dichroic

You can buy some dichroic paper and paper punches. I have used the paper with butterfly and dragonfly puches and fused it to my glass. They turn out very nice.

anitac

why don't you carve the

why don't you carve the letter away?

petra kaiser - www.kaiserlee.com

 