This site is brought to you by Helios Kiln Glass Studio in Austin, TX.
Murano sheet glass firing schedule?
Submitted by bybee2130 on Mon, 03/15/2010 - 08:42.
I´m looking for firing schedules (full fuse and tac-fuse) for COE 104 - glass (Murano sheets). If possible in Celsius (but Fahrenheit is possible too)!
Used to work with bullseye till now.


Moretti Rods information
Moretti Rods
information from yglass.com.
Specifications: Coefficient of Expansion (C.O.E): 104x10C
Rods per pound:7-8 Rod
Length: Approx 39" (1meter)
Rod Diameter:5-6mm
Strain Point: 840 Farenhiet 448C
Working Temprature: 1700 Farenhiet 926C
Annealing Range: 920-928 Farenheit 493 – 498C
Softening Point: 1050 Farenheit. 565C
This is for rods and does not give the full fuse temperature, but I would guess it would be 5-10C below S96.
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/