Hi, I have a SC3 Paragon Kiln which is in Celsius & was hoping someone might have some Ramp..., Temperatures... & hold time schedules for slumping or melting a glass beer bottle... any help would be apprecated....  Cheers Jenny..Undecided

Hi Jenny - sorry for the

Hi Jenny - sorry for the long delayed response.  Your post was in the forum help section (intended for help on using this website) so I never saw it.

I use the "Soft Fuse/3 layer" schedule on this site to slump bottles with consistent success.  Just click "Firing Schedules" under the tools menu above.

----------------------
Paul
FusedGlass.Org
Helios Kiln Glass Studio
PaulTarlow.com

 